Grade equivalence

Cross-reference a grade across UNS, ASTM/AISI, EN (W.Nr.) and JIS. Type anything — a grade name, a UNS number or a material number — and the table filters live.

64 grades listed

Indicative cross-references for guidance only. Always confirm against the governing standard and the Material Test Certificate. A dash means we are not confident of the cross-reference and will not guess.

Click a column heading to sort
Notes
304S304003041.4301 · X5CrNi18-10SUS 304General purpose austenitic
304LS30403304L1.4307 · X2CrNi18-9SUS 304LLow carbon, weldable without sensitisation
316S316003161.4401SUS 316Molybdenum bearing, better pitting resistance
316LS31603316L1.4404SUS 316LThe default process grade
316TiS31635316Ti1.4571SUS 316TiTitanium stabilised for elevated temperature
317LS31703317L1.4438SUS 317LHigher Mo than 316L
321S321003211.4541SUS 321Titanium stabilised, resists sensitisation
347S347003471.4550SUS 347Niobium stabilised
310SS31008310S1.4845SUS 310SHeat resisting to about 1050 °C
904LN08904904L1.4539SUS 890LHigh Ni-Mo-Cu, sulphuric acid service
202S202002021.4373SUS 202Manganese substituted austenitic
409S409004091.4512SUH 409Ferritic, automotive exhaust
410S410004101.4006SUS 410Martensitic, hardenable
420S420004201.4021SUS 420J1Martensitic, higher carbon
430FS43020430F1.4104SUS 430FFree machining ferritic
17-4 PHS174006301.4542SUS 630Precipitation hardening, high strength
15-5 PHS15500XM-121.4545PH grade with improved toughness
Nitronic 50S20910XM-19High strength austenitic, non-magnetic
Nitronic 60S21800Galling and wear resistant
Duplex 2205S32205A240 S322051.4462SUS 329J3LPREN ≈ 35; the modern 2205
Duplex (older 2205)S31803A240 S318031.4462Wider composition range than S32205
Super Duplex 2507S32750A240 S327501.4410PREN ≈ 42
Super DuplexS32760A240 S327601.4501Zeron 100 type
Alloy 20N08020B4632.4660Sulphuric acid service
Sanicro 28N080281.4563High alloy austenitic, phosphoric acid
2RE69S310501.4466Urea grade — confirm against the mill specification
2RE10Urea grade — confirm against the mill specification
Inconel 600N06600B166 / B1672.4816NCF 600Ni-Cr, high temperature
Inconel 625N06625B443 / B4442.4856NCF 625Ni-Cr-Mo-Nb, very wide corrosion range
Inconel 718N07718B6372.4668Age hardening, high strength
Incoloy 800N08800B407 / B4091.4876NCF 800Fe-Ni-Cr, heat resisting
Incoloy 825N08825B423 / B4242.4858NCF 825Ni-Fe-Cr-Mo-Cu, acid service
Incoloy 925N09925Age hardenable 825 variant
Monel 400N04400B127 / B1652.4360NW 4400Ni-Cu, seawater and HF service
Monel K500N05500B8652.4375Age hardened Monel
Hastelloy C276N10276B575 / B6222.4819Ni-Mo-Cr, reducing and oxidising acids
Hastelloy C22N06022B575 / B6222.4602Improved oxidising resistance over C276
Titanium Gr 2R50400B265 / B3383.7035Commercially pure, seawater and chlorides
Titanium Gr 5R56400B265 (Ti-6Al-4V)3.7165Alpha-beta alloy, structural
Titanium Gr 7R52400B2653.7235Palladium bearing, reducing acids
Titanium Gr 12R53400B265Improved crevice corrosion resistance
Cupro-Nickel 90/10C70600B111 / B4662.0872 · CuNi10Fe1MnSeawater, biofouling resistant
Cupro-Nickel 70/30C71500B111 / B4662.0882 · CuNi30Mn1FeHigher velocity seawater duty
Copper C110 (ETP)C11000B1522.0065 · Cu-ETPC1100Electrolytic tough pitch
Copper C101 (OF)C10100B1522.0040 · Cu-OFC1011Oxygen free
Cu-DHPC12200B75 / B882.0090C1220Phosphorus deoxidised, brazeable
Free Cutting Brass C360C36000B162.0401 · CuZn39Pb3C3604High-speed machining
Admiralty BrassC44300B1112.0470C4430Condenser tube
Naval BrassC46400B212.0530C4640Marine fittings
Cartridge BrassC26000B192.0265 · CuZn30C2600Deep drawing
Phosphor BronzeC51000B1032.1020C5101Springs and bearings
Aluminium Bronze C63000C63000B1502.0966High strength, marine
Zirconium 702R60702B523 / B550Strong acid service
TantalumR05200B708Near universal acid resistance
NiobiumR04200B394Reactive metal, specialist duty
SA 516 Gr 60K02100SA / A516 Gr 601.0425 · P265GH (near)Boiler quality plate
SA 516 Gr 70K02700SA / A516 Gr 701.0473 · P355GH (near)Boiler quality plate
S355J2+NA572 Gr 50 (near)1.0577Structural, impact tested at −20 °C
S690QLA514 (near)1.8928Quenched and tempered high strength
S700MC1.8974Thermomechanically rolled
Corten AK11430A242 / A5881.8945 · S355J0WPWeathering steel
IS 2062 E2501.0038 · S235JR (near)Indian structural standard
IS 2062 E3501.0045 · S355JR (near)Indian structural standard
IS 2062 E510Indian structural standard, high strength